Dimension
Property | Value |
---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation A50 | 23.0 °C | 8 % Show Supplier Material materials with Elongation A50 of 8 % | Min. |
Tensile strength | 23.0 °C | 190 MPa Show Supplier Material materials with Tensile strength of 190 MPa | |
Yield strength Rp0.2 | 23.0 °C | 160 MPa Show Supplier Material materials with Yield strength Rp0.2 of 160 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.36E-5 1/K | for 20-100°C |
Melting point | 633 °C Show Supplier Material materials with Melting point of 633 °C | Mean | |
Specific heat capacity | 23.0 °C | 889 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 889 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 160 W/(m·K) Show Supplier Material materials with Thermal conductivity of 160 W/(m·K) | After brazing, calculated from electric resistivity data measured at room temperature |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | 3.4E-8 - 4.3E-8 Ω·m Show Supplier Material materials with Electrical resistivity of 3.4E-8 - 4.3E-8 Ω·m | Changes depending on temper |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Processing history | Temper: H24 |