Dimension
Property | Value |
---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> |
Mechanical
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.36e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.36e-05 1/K | for 20-100°C |
Melting point | 633 °C Show Supplier Material materials with Melting point of 633 °C | Mean |
Electrical
Property | Value | Comment |
---|---|---|
Corrosion potential | -695 mV Show Supplier Material materials with Corrosion potential of -695 mV | |
Electrical resistivity | 3.4e-08 - 4.3e-08 Ω·m Show Supplier Material materials with Electrical resistivity of 3.4e-08 - 4.3e-08 Ω·m | Changes depending on temper |
Chemical properties
Property | Value |
---|---|
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Corrosion properties | Improved corossion resistance | |
Processing history | Temper: H24 |