Aluminium Tube Alloys (Welded & Folded) MC96 H24

Want to keep this datasheet? Save it now in your required format

Description

Multiclad

This material data has been provided by Gränges.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

<p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p>

Mechanical

PropertyValueTemperatureComment

Elongation A50

8 %

Show Supplier Material materials with Elongation A50 of 8 % at 23.0 °C

23.0 °C

Min.

Tensile strength

190 MPa

Show Supplier Material materials with Tensile strength of 190 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

160 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 160 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

2.36E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.36E-5 1/K at 23.0 °C

23.0 °C

for 20-100°C

Specific heat capacity

889 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 889 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

160 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 160 W/(m·K) at 23.0 °C

23.0 °C

After brazing, calculated from electric resistivity data measured at room temperature

Electrical

PropertyValueTemperatureComment

Electrical resistivity

3.4E-8 - 4.3E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.4E-8 - 4.3E-8 Ω·m at 23.0 °C

23.0 °C

Changes depending on temper

Technological properties

Property
Application areas

Automotive, Heat Exchangers

Processing history

Temper: H24