Aluminium Alloy Plate, Sidesuport, Header, Tube plate (O) FA 7021

Want to keep this datasheet? Save it now in your required format

Description

Strong and corrosion resistant material for header and plate applications


Use the URL below for more information:

Gränges products

Equivalent Materials

This material data has been provided by Gränges.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

<p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p>

Mechanical

PropertyTemperatureValueComment

Elongation A50

23.0 °C

20 %

Show Supplier Material materials with Elongation A50 of 20 %

Min.

Tensile strength

23.0 °C

110 MPa

Show Supplier Material materials with Tensile strength of 110 MPa

Yield strength Rp0.2

23.0 °C

50 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 50 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.36E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.36E-5 1/K

for 20-100°C

Melting point

607 °C

Show Supplier Material materials with Melting point of 607 °C

Mean

Specific heat capacity

23.0 °C

889 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 889 J/(kg·K)

Thermal conductivity

23.0 °C

160 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 160 W/(m·K)

After brazing, calculated from electric resistivity data measured at room temperature

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

3.4E-8 - 4.3E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.4E-8 - 4.3E-8 Ω·m

Changes depending on temper

Chemical properties

PropertyValue

Zinc

0.1 %

Show Supplier Material materials with Zinc of 0.1 %

Technological properties

Property
Application areas

Automotive, Heat Exchangers

Processing history

Temper: O