Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Find Materials
Categories
Aluminium Alloy Braze clad - CAB FA 6651
This material data has been provided by Gränges.
All categories
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.36E-5 1/K |
Melting point | 565 °C Show Supplier Material materials with Melting point of 565 °C | |
Specific heat capacity | 23.0 °C | 889 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 889 J/(kg·K) |
Chemical properties
Property | Value |
---|---|
Zinc | 4.1 - 4.9 % Show Supplier Material materials with Zinc of 4.1 - 4.9 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.