General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.54 g/cm³ Show Supplier Material materials with Density of 2.54 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 80 GPa Show Supplier Material materials with Elastic modulus of 80 GPa |
Elongation A50 | 23.0 °C | 2 % Show Supplier Material materials with Elongation A50 of 2 % |
Hardness, Vickers, 30 | 23.0 °C | 58 [-] Show Supplier Material materials with Hardness, Vickers, 30 of 58 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.46E-5 - 1.56E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.46E-5 - 1.56E-5 1/K |
Melting point | 575.9 °C Show Supplier Material materials with Melting point of 575.9 °C | |
Specific heat capacity | 23.0 °C | 850 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 850 J/(kg·K) |
Thermal conductivity | 30.0 °C | 152.4 W/(m·K) Show Supplier Material materials with Thermal conductivity of 152.4 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.57E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.57E+7 S/m |
Chemical properties
Property | Value |
---|---|
Silicon | 35 % Show Supplier Material materials with Silicon of 35 % |
Technological properties
Property | ||
---|---|---|
Application areas | Industrial Applications, Linear Technology | |
Processing history | Spray Compaction, Extrusion |