General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.79 g/cm³ Show Supplier Material materials with Density of 2.79 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 90 GPa Show Supplier Material materials with Elastic modulus of 90 GPa |
Elongation A50 | 23.0 °C | 0.8 % Show Supplier Material materials with Elongation A50 of 0.8 % |
Hardness, Vickers, 30 | 23.0 °C | 160 [-] Show Supplier Material materials with Hardness, Vickers, 30 of 160 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.52E-5 - 1.62E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.52E-5 - 1.62E-5 1/K |
Melting point | 539.3 °C Show Supplier Material materials with Melting point of 539.3 °C | |
Specific heat capacity | 23.0 °C | 820 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 820 J/(kg·K) |
Thermal conductivity | 30.0 °C | 95.5 W/(m·K) Show Supplier Material materials with Thermal conductivity of 95.5 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.01E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.01E+7 S/m |
Chemical properties
Property | Value |
---|---|
Chromium | 1 % Show Supplier Material materials with Chromium of 1 % |
Copper | 1 % Show Supplier Material materials with Copper of 1 % |
Iron | 4 % Show Supplier Material materials with Iron of 4 % |
Magnesium | 1 % Show Supplier Material materials with Magnesium of 1 % |
Manganese | 1 % Show Supplier Material materials with Manganese of 1 % |
Nickel | 3 % Show Supplier Material materials with Nickel of 3 % |
Silicon | 25 % Show Supplier Material materials with Silicon of 25 % |
Titanium | 1 % Show Supplier Material materials with Titanium of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | High Temperature-High Strength Industrial and Automotive | |
Processing history | Spray Compaction, Extrusion |