General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Density | 2.413 - 2.667 g/cm³ Show Supplier Material materials with Density of 2.413 - 2.667 g/cm³ | ||
Mean Roughness | 8 μm Show Supplier Material materials with Mean Roughness of 8 μm | DIN EN ISO 16610-21 | |
Mean Roughness Depth | 50 μm Show Supplier Material materials with Mean Roughness Depth of 50 μm | DIN EN ISO 16610-21 | |
Relative density | 99.8 [-] Show Supplier Material materials with Relative density of 99.8 [-] | min. | Optical density determination at test specimen by light microscopy |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elastic modulus | 90 GPa Show Supplier Material materials with Elastic modulus of 90 GPa | min. | |
Elongation | 1.5 % Show Supplier Material materials with Elongation of 1.5 % | min. | |
Tensile strength | 200 MPa Show Supplier Material materials with Tensile strength of 200 MPa | DIN EN ISO 6892-1 Method B | min. |
Yield strength | 115 MPa Show Supplier Material materials with Yield strength of 115 MPa | min., RP02 |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.46e-05 - 1.56e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.46e-05 - 1.56e-05 1/K | for 20-100°C |
1.55e-05 - 1.65e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.55e-05 - 1.65e-05 1/K | for 20-200°C | |
1.63e-05 - 1.73e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.63e-05 - 1.73e-05 1/K | for 20-300°C |
Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Silicon | 34 - 36 % Show Supplier Material materials with Silicon of 34 - 36 % |
Technological properties
Property | ||
---|---|---|
Application areas | The material is used in a wide range of industries such as linear technology, optical industry and aerospace. Typical applications include housings, moving components and other lightweight applications. | |
Other | The properties in this material data sheet reflect minimum values that are achieved when printing S220 powder on an industrial Additive Manufacturing (AM) machine. The machine used is a Concept Laser M2, Laser Powder Bed Fusion category. |