TPU 8301

Alternative and trade names
8301
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 8301 product is engineering thermoplastic polyurethane resin. It exhibits excellent tensile and flexural strength, toughness, abrasive resistance, good fatigue resistance, solvent resistance, and maintenance of good physical properties under UV exposure. The product can be injection molded and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elastic modulus

1.88 GPa

Show Supplier Material materials with Elastic modulus of 1.88 GPa

ASTM D638

Elongation

45.0 %

Show Supplier Material materials with Elongation of 45.0 %

ASTM D638

Flexural modulus

2.0 GPa

Show Supplier Material materials with Flexural modulus of 2.0 GPa

ASTM D790

Flexural strength

110.0 MPa

Show Supplier Material materials with Flexural strength of 110.0 MPa

ASTM D790

Hardness, Shore D

85.0 [-]

Show Supplier Material materials with Hardness, Shore D of 85.0 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

113 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 113 J/m

ASTM D256

Tensile strength

86.0 MPa

Show Supplier Material materials with Tensile strength of 86.0 MPa

ASTM D638

Thermal

PropertyValuePressureComment

Heat deflection temperature

132.0 °C

Show Supplier Material materials with Heat deflection temperature of 132.0 °C

0.45 MPa

ASTM D648

Vicat softening temperature

142.0 °C

Show Supplier Material materials with Vicat softening temperature of 142.0 °C

ASTM D1525

Technological properties

Property
Application areas

Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products.