ISOTHANE 8101-B is a polyether based thermoplastic polyurethane having excellent bio-compatibility, hydrolytic resistance, fungus resistance and low temperature performance properties. This product is used for biomedical and drug administration applications. ISOTHANE 8101-B can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

125.0 %

Show Supplier Material materials with Elongation of 125.0 %

ASTM D638

Flexural modulus

1.73 GPa

Show Supplier Material materials with Flexural modulus of 1.73 GPa

ASTM D790

Hardness, Shore D

80.0 [-]

Show Supplier Material materials with Hardness, Shore D of 80.0 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

117 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117 J/m

ASTM D256

Tensile strength

75.0 MPa

Show Supplier Material materials with Tensile strength of 75.0 MPa

ASTM D638

Thermal

PropertyValuePressureComment

Heat deflection temperature

93.0 °C

Show Supplier Material materials with Heat deflection temperature of 93.0 °C

0.45 MPa

ASTM D648

Vicat softening temperature

100.0 °C

Show Supplier Material materials with Vicat softening temperature of 100.0 °C

ASTM D1525