TPU 5090A

Alternative and trade names
5090A
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 5090A is a polyether based thermoplastic polyurethane having excellent bio-compatibility, hydrolytic resistance, fungus resistance and low temperature performance properties. This product is used for biomedical and drug administration applications. ISOTHANE 5090A can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.12 g/cm³

Show Supplier Material materials with Density of 1.12 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

490.0 %

Show Supplier Material materials with Elongation of 490.0 %

ASTM D412

Flexural modulus

0.07200000000000001 GPa

Show Supplier Material materials with Flexural modulus of 0.07200000000000001 GPa

ASTM D790

Hardness, Shore A

90.0 [-]

Show Supplier Material materials with Hardness, Shore A of 90.0 [-]

ASTM D2240

Tear strength

176.0 kN/m

Show Supplier Material materials with Tear strength of 176.0 kN/m

ASTM D624

Tensile strength

51.0 MPa

Show Supplier Material materials with Tensile strength of 51.0 MPa

ASTM D412

Technological properties

Property
Application areas

Medical Tubing and Medical Disposable Applications.