TPU B1095A

Alternative and trade names
B1095A
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE B1095A is a polyester based thermoplastic polyurethane having high elasticity and recovery. It has excellent toughness, abrasive resistance, and solvent resistance. ISOTHANE B1095A can be processed by injection molding, blow molding, and extrusion.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.22 g/cm³

Show Supplier Material materials with Density of 1.22 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

600.0 %

Show Supplier Material materials with Elongation of 600.0 %

ASTM D412

Hardness, Shore A

95.0 [-]

Show Supplier Material materials with Hardness, Shore A of 95.0 [-]

ASTM D2240

Tear strength

180.0 kN/m

Show Supplier Material materials with Tear strength of 180.0 kN/m

ASTM D624

Tensile strength

60.0 MPa

Show Supplier Material materials with Tensile strength of 60.0 MPa

ASTM D412

Technological properties

Property
Application areas

Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods.