TPU 3085AU-EJ

Alternative and trade names
3085AU-EJ
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 3085AU-EJ is a polyether based thermoplastic polyurethane having high elasticity and recovery. It has excellent mechanical properties and good damping characteristics. ISOTHANE 3085AU-EJ can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.12 g/cm³

Show Supplier Material materials with Density of 1.12 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

700.0 %

Show Supplier Material materials with Elongation of 700.0 %

ASTM D412

Hardness, Shore A

85.0 [-]

Show Supplier Material materials with Hardness, Shore A of 85.0 [-]

ASTM D2240

Tear strength

110.0 kN/m

Show Supplier Material materials with Tear strength of 110.0 kN/m

ASTM D624

Tensile strength

37.0 MPa

Show Supplier Material materials with Tensile strength of 37.0 MPa

ASTM D412

Technological properties

Property
Application areas

ISOTHANE 3000 Series-General Purpose Grade