TPU 1075A

Alternative and trade names
1075A
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 1075A is a polyester based thermoplastic polyurethane. This exhibits good toughness, solvent resistance, easy processing, and high transparency. ISOTHANE 1075A can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

800.0 %

Show Supplier Material materials with Elongation of 800.0 %

ASTM D412

Hardness, Shore A

75.0 [-]

Show Supplier Material materials with Hardness, Shore A of 75.0 [-]

ASTM D2240

Tear strength

100.0 kN/m

Show Supplier Material materials with Tear strength of 100.0 kN/m

ASTM D624

Tensile strength

31.0 MPa

Show Supplier Material materials with Tensile strength of 31.0 MPa

ASTM D412

Technological properties

Property
Application areas

Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods.