TPU 1170D

Alternative and trade names
1170D
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 1170D is a polyester based thermoplastic polyurethane. This exhibits good toughness, solvent resistance, easy processing, and high transparency. ISOTHANE 1170D can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.23 g/cm³

Show Supplier Material materials with Density of 1.23 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

310.0 %

Show Supplier Material materials with Elongation of 310.0 %

ASTM D412

Hardness, Shore D

70.0 [-]

Show Supplier Material materials with Hardness, Shore D of 70.0 [-]

ASTM D2240

Tear strength

220.0 kN/m

Show Supplier Material materials with Tear strength of 220.0 kN/m

ASTM D624

Tensile strength

40.0 MPa

Show Supplier Material materials with Tensile strength of 40.0 MPa

ASTM D412

Technological properties

Property
Application areas

Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods.