Description

ISOTHANE 8102 is an engineering thermoplastic polyurethane. ISOTHANE 102 exhibit excellent tensile and flexural strength, toughness, abrasive resistance, good fatigue resistance, solvent resistance, and maintenance of good physical properties under UV exposure. ISOTHANE 8102 can be injection molded and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elastic modulus

1.08 GPa

Show Supplier Material materials with Elastic modulus of 1.08 GPa

ASTM D638

Elongation

150.0 %

Show Supplier Material materials with Elongation of 150.0 %

ASTM D638

Flexural modulus

1.37 GPa

Show Supplier Material materials with Flexural modulus of 1.37 GPa

ASTM D790

Flexural strength

74.0 MPa

Show Supplier Material materials with Flexural strength of 74.0 MPa

ASTM D790

Hardness, Shore D

76.0 [-]

Show Supplier Material materials with Hardness, Shore D of 76.0 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

1060 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 1060 J/m

ASTM D256

Tensile strength

60.0 MPa

Show Supplier Material materials with Tensile strength of 60.0 MPa

ASTM D638

Thermal

PropertyValuePressureComment

Heat deflection temperature

90.0 °C

Show Supplier Material materials with Heat deflection temperature of 90.0 °C

0.45 MPa

ASTM D648

Vicat softening temperature

98.0 °C

Show Supplier Material materials with Vicat softening temperature of 98.0 °C

ASTM D1525

Technological properties

Property
Application areas

Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products.