TPU 8303

Alternative and trade names
8303
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 8303 is an engineering thermoplastic polyurethane. ISOTHANE 8303 exhibit excellent tensile and flexural strength, toughness, abrasive resistance, good fatigue resistance, solvent resistance, and maintenance of good physical properties under UV exposure. ISOTHANE 8303 can be injection molded and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.35 GPa

Show Supplier Material materials with Elastic modulus of 1.35 GPa

ASTM D638

Elongation

23.0 °C

92 %

Show Supplier Material materials with Elongation of 92 %

ASTM D638

Flexural modulus

23.0 °C

1.58 GPa

Show Supplier Material materials with Flexural modulus of 1.58 GPa

ASTM D790

Flexural strength

23.0 °C

91 MPa

Show Supplier Material materials with Flexural strength of 91 MPa

ASTM D790

Hardness, Shore D

23.0 °C

78 [-]

Show Supplier Material materials with Hardness, Shore D of 78 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

646 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 646 J/m

ASTM D256

Tensile strength

23.0 °C

67 MPa

Show Supplier Material materials with Tensile strength of 67 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

110 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 110 °C

ASTM D648

Vicat softening temperature

129 °C

Show Supplier Material materials with Vicat softening temperature of 129 °C

ASTM D1525

Technological properties

Property