ISOTHANE 2090A-M is a polyester poly(caprolactone)ester based thermoplastic polyurethane. ISOTHANE 2090A-M exhibits excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stability. ISOTHANE 2090A-M can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Compression set

23 °C

20 [-]

Show Supplier Material materials with Compression set of 20 [-]

ASTM D395, for 22hrs

70 °C

28 [-]

Show Supplier Material materials with Compression set of 28 [-]

ASTM D395, for 22hrs

Elongation

450.0 %

Show Supplier Material materials with Elongation of 450.0 %

ASTM D412

Hardness, Shore A

91.0 [-]

Show Supplier Material materials with Hardness, Shore A of 91.0 [-]

ASTM D2240

Tear strength

120.0 kN/m

Show Supplier Material materials with Tear strength of 120.0 kN/m

ASTM D624

Tensile strength

56.0 MPa

Show Supplier Material materials with Tensile strength of 56.0 MPa