PCL 2090A-MH

Alternative and trade names
2090A-MH
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 2090A-MH is a polyester poly(caprolactone)ester based thermoplastic polyurethane. ISOTHANE 2090A-MH exhibits excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stability. ISOTHANE 2090A-MH can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Compression set

100.0 °C

33 [-]

Show Supplier Material materials with Compression set of 33 [-]

ASTM D395, for 22hrs

Elongation

23.0 °C

580 %

Show Supplier Material materials with Elongation of 580 %

ASTM D412

Hardness, Shore A

23.0 °C

90 [-]

Show Supplier Material materials with Hardness, Shore A of 90 [-]

ASTM D2240

Tear strength

23.0 °C

130 kN/m

Show Supplier Material materials with Tear strength of 130 kN/m

ASTM D624

Tensile strength

23.0 °C

30 MPa

Show Supplier Material materials with Tensile strength of 30 MPa

ASTM D638

Technological properties

Property
Application areas

Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods.