Description

ISOTHANE 3075A is a polyether based thermoplastic polyurethane. ISOTHANE 3075A exhibits excellent mechanical properties, hydrolytic resistance, fungus resistance, and low temperature performance properties. ISOTHANE 3075A can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.11 g/cm³

Show Supplier Material materials with Density of 1.11 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

930.0 %

Show Supplier Material materials with Elongation of 930.0 %

ASTM D412

Hardness, Shore A

73.0 [-]

Show Supplier Material materials with Hardness, Shore A of 73.0 [-]

ASTM D2240

Tear strength

86.0 kN/m

Show Supplier Material materials with Tear strength of 86.0 kN/m

ASTM D624

Tensile strength

21.0 MPa

Show Supplier Material materials with Tensile strength of 21.0 MPa

ASTM D412

Technological properties

Property
Application areas

Apparel Applications And Outdoor Applications.