Description

ISOTHANE 3095AU is a polyether based thermoplastic polyurethane. ISOTHANE 3095AU exhibits excellent mechanical properties, hydrolytic resistance, fungus resistance, and low temperature performance properties. ISOTHANE 3095AU can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.15 g/cm³

Show Supplier Material materials with Density of 1.15 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

570.0 %

Show Supplier Material materials with Elongation of 570.0 %

ASTM D412

Hardness, Shore A

93.0 [-]

Show Supplier Material materials with Hardness, Shore A of 93.0 [-]

ASTM D2240

Tear strength

136.0 kN/m

Show Supplier Material materials with Tear strength of 136.0 kN/m

ASTM D624

Tensile strength

52.0 MPa

Show Supplier Material materials with Tensile strength of 52.0 MPa

ASTM D412

Technological properties

Property
Application areas

Apparel Applications And Outdoor Applications.