TPU 1690A-E6

Alternative and trade names
1690A-E6
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 1690A-E6 is a polyether based thermoplastic polyurethane with good balanced qualities. ISOTHANE 1690A-E6 exhibits excellent high moisture vapor transmission. ISOTHANE 1690A-E6 can be processed by blown film extrusion.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

700 %

Show Supplier Material materials with Elongation of 700 %

ASTM D412

Hardness, Shore A

23.0 °C

89 [-]

Show Supplier Material materials with Hardness, Shore A of 89 [-]

ASTM D2240

Tear strength

23.0 °C

110 kN/m

Show Supplier Material materials with Tear strength of 110 kN/m

ASTM D624

Tensile strength

23.0 °C

26 MPa

Show Supplier Material materials with Tensile strength of 26 MPa

ASTM D412

Technological properties

Property
Application areas

Apparel Applications.