Description

ISOTHANE 7285A is an aliphatic polycaprolactone based thermoplastic polyurethane having high elasticity and transparency. It has excellent mechanical properties, abrasion resistance, hydrolysis resistance and no yellowing on exposure to UV light. ISOTHANE 7285A can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.12 g/cm³

Show Supplier Material materials with Density of 1.12 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

650.0 %

Show Supplier Material materials with Elongation of 650.0 %

ASTM D412

Hardness, Shore A

85.0 [-]

Show Supplier Material materials with Hardness, Shore A of 85.0 [-]

ASTM D2240

Tear strength

135.0 kN/m

Show Supplier Material materials with Tear strength of 135.0 kN/m

ASTM D624

Tensile strength

23.0 MPa

Show Supplier Material materials with Tensile strength of 23.0 MPa

ASTM D412

Technological properties

Property
Application areas

Automotive Protective Films and Smart Wearable Devices