TPU 7385A-E

Alternative and trade names
7385A-E
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 7385A-E is an aliphatic polycaprolactone based thermoplastic polyurethane having high elasticity and transparency. It has excellent mechanical properties, abrasion resistance, hydrolysis resistance and no yellowing on exposure to UV light. ISOTHANE 7385A-E can be processed by extrusion and injection molding.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.08 g/cm³

Show Supplier Material materials with Density of 1.08 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

400.0 %

Show Supplier Material materials with Elongation of 400.0 %

ASTM D412

Hardness, Shore A

85.0 [-]

Show Supplier Material materials with Hardness, Shore A of 85.0 [-]

ASTM D2240

Tear strength

115.0 kN/m

Show Supplier Material materials with Tear strength of 115.0 kN/m

ASTM D624

Tensile strength

43.0 MPa

Show Supplier Material materials with Tensile strength of 43.0 MPa

ASTM D412

Technological properties

Property
Application areas

Automotive Protective Films and Smart Wearable Devices