TPU 3085A-FR

Alternative and trade names
TPU FR
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 3085A-FR have good initial adhesive strength, fast crystallization, good solubility, good washing durability and freezing resistance. Viscosity ranges from 150~2800cps (15% MEK Solution), and viscosity could be customized for different viscosity. ISOTHANE 3085A-FR exhibits good adhesive with TPU, PVC, polyester fabric, leather and other materials.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.15 g/cm³

Show Supplier Material materials with Density of 1.15 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

570 %

Show Supplier Material materials with Elongation of 570 %

ASTM D412

Hardness, Shore A

23.0 °C

85 [-]

Show Supplier Material materials with Hardness, Shore A of 85 [-]

ASTM D2240

Tear strength

23.0 °C

130 kN/m

Show Supplier Material materials with Tear strength of 130 kN/m

ASTM D624

Tensile strength

23.0 °C

29 MPa

Show Supplier Material materials with Tensile strength of 29 MPa

ASTM D412

Thermal

PropertyValue

Flammability

UL94 V0 (2mm)

Technological properties

Property
Application areas

Building/Construction, Mining, Wire and Cables