TPU 5085A

Alternative and trade names
5085A
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 5085A is a polyether based thermoplastic polyurethane having excellent bio-compatibility, hydrolytic resistance, fungus resistance and low temperature performance properties. This product is used for biomedical and drug administration applications. ISOTHANE 5085A can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

540 %

Show Supplier Material materials with Elongation of 540 %

ASTM D412

Flexural modulus

23.0 °C

0.04 GPa

Show Supplier Material materials with Flexural modulus of 0.04 GPa

ASTM D790

Hardness, Shore A

23.0 °C

85 [-]

Show Supplier Material materials with Hardness, Shore A of 85 [-]

ASTM D2240

Tear strength

23.0 °C

90 kN/m

Show Supplier Material materials with Tear strength of 90 kN/m

ASTM D624

Tensile strength

23.0 °C

39 MPa

Show Supplier Material materials with Tensile strength of 39 MPa

ASTM D412

Technological properties

Property
Application areas

Medical Tubing and Medical Disposable Applications.

Certifications

Bio-compatibility according to USP class VI