TPU 5095A

Alternative and trade names
5095A
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 5095A is a polyether based thermoplastic polyurethane having excellent bio-compatibility, hydrolytic resistance, fungus resistance and low temperature performance properties. This product is used for biomedical and drug administration applications. ISOTHANE 5095A can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.15 g/cm³

Show Supplier Material materials with Density of 1.15 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

438.0 %

Show Supplier Material materials with Elongation of 438.0 %

ASTM D412

Flexural modulus

0.096 GPa

Show Supplier Material materials with Flexural modulus of 0.096 GPa

ASTM D790

Hardness, Shore A

95.0 [-]

Show Supplier Material materials with Hardness, Shore A of 95.0 [-]

ASTM D2240

Tear strength

190.0 kN/m

Show Supplier Material materials with Tear strength of 190.0 kN/m

ASTM D624

Tensile strength

51.0 MPa

Show Supplier Material materials with Tensile strength of 51.0 MPa

ASTM D412

Technological properties

Property
Application areas

Medical Tubing and Medical Disposable Applications.

Certifications

Bio-compatibility according to USP class VI