TPU 8102-B

Alternative and trade names
8102-B
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 8102-B is a polyether based thermoplastic polyurethane having excellent bio-compatibility, hydrolytic resistance, fungus resistance and low temperature performance properties. This product is used for biomedical and drug administration applications. ISOTHANE 8102-B can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

150.0 %

Show Supplier Material materials with Elongation of 150.0 %

ASTM D412

Flexural modulus

1.37 GPa

Show Supplier Material materials with Flexural modulus of 1.37 GPa

ASTM D790

Hardness, Shore D

76.0 [-]

Show Supplier Material materials with Hardness, Shore D of 76.0 [-]

ASTM D2240

Tensile strength

60.0 MPa

Show Supplier Material materials with Tensile strength of 60.0 MPa

ASTM D412

Technological properties

Property
Application areas

Medical Tubing and Medical Disposable Applications.

Certifications

Bio-compatibility according to USP class VI