PA LGN401

Alternative and trade names
LGN401
Want to keep this datasheet? Save it now in your required format

Description

Excellent strength, Heat resistance, Dimensional stability

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.45 g/cm³

Show Supplier Material materials with Density of 1.45 g/cm³

Mechanical

PropertyValueComment

Elongation

2.0 %

Show Supplier Material materials with Elongation of 2.0 %

Flexural modulus

11.772 GPa

Show Supplier Material materials with Flexural modulus of 11.772 GPa

Flexural strength

294.0 MPa

Show Supplier Material materials with Flexural strength of 294.0 MPa

Impact strength, Izod notched, ASTM

294 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 294 J/m

ASTM D256

Tensile strength

196.0 MPa

Show Supplier Material materials with Tensile strength of 196.0 MPa

Rheological Properties

PropertyValue

Shrinkage

0.1 %

Show Supplier Material materials with Shrinkage of 0.1 %

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

Technological properties

Property
Application areas

Mechanical Parts, Sports Equipment