PA LGN501

Alternative and trade names
LGN501
Want to keep this datasheet? Save it now in your required format

Description

Excellent strength, Heat resistance, Dimensional stability

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.57 g/cm³

Show Supplier Material materials with Density of 1.57 g/cm³

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

Flexural modulus

23.0 °C

13.74 GPa

Show Supplier Material materials with Flexural modulus of 13.74 GPa

Flexural strength

23.0 °C

344 MPa

Show Supplier Material materials with Flexural strength of 344 MPa

Impact strength, Izod notched, ASTM

23.0 °C

400 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 400 J/m

ASTM D256

Tensile strength

23.0 °C

216 MPa

Show Supplier Material materials with Tensile strength of 216 MPa

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.05 - 0.2 %

Show Supplier Material materials with Shrinkage of 0.05 - 0.2 %

Technological properties

Property
Application areas

Mechanical Parts, Sports Equipment