PA LGN402

Alternative and trade names
LGN402
Want to keep this datasheet? Save it now in your required format

Description

Excellent strength, Heat resistance, Dimensional stability

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.45 g/cm³

Show Supplier Material materials with Density of 1.45 g/cm³

Mechanical

PropertyValueComment

Elongation

2.0 %

Show Supplier Material materials with Elongation of 2.0 %

Flexural modulus

11.776 GPa

Show Supplier Material materials with Flexural modulus of 11.776 GPa

Flexural strength

304.0 MPa

Show Supplier Material materials with Flexural strength of 304.0 MPa

Impact strength, Izod notched, ASTM

200 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 200 J/m

ASTM D256

Tensile strength

216.0 MPa

Show Supplier Material materials with Tensile strength of 216.0 MPa

Rheological Properties

PropertyValue

Shrinkage

0.05 %

Show Supplier Material materials with Shrinkage of 0.05 %

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %