Description

Excellent strength, Heat resistance, Dimensional stability

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.59 g/cm³

Show Supplier Material materials with Density of 1.59 g/cm³

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

Flexural modulus

23.0 °C

18.65 GPa

Show Supplier Material materials with Flexural modulus of 18.65 GPa

Flexural strength

23.0 °C

363 MPa

Show Supplier Material materials with Flexural strength of 363 MPa

Impact strength, Izod notched, ASTM

23.0 °C

350 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 350 J/m

ASTM D256

Tensile strength

23.0 °C

245 MPa

Show Supplier Material materials with Tensile strength of 245 MPa

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.05 - 0.2 %

Show Supplier Material materials with Shrinkage of 0.05 - 0.2 %

Technological properties

Property
Application areas

Mechanical Parts, Sports Equipment