TPU 8102LGF50

Alternative and trade names
8102LGF50
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 8102LGF50 is a long glass fiber reinforced. ISOTHANE 8102LGF50 exhibits excellent tensile and flexural strength, toughness,abrasive resistance, high rigidity, and maintenance of good physical properties under UV exposure. ISOTHANE 8102LGF50 can be injection molded and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.6 g/cm³

Show Supplier Material materials with Density of 1.6 g/cm³

Mechanical

PropertyValue

Flexural modulus

12.3 GPa

Show Supplier Material materials with Flexural modulus of 12.3 GPa

Flexural strength

315.0 MPa

Show Supplier Material materials with Flexural strength of 315.0 MPa

Impact strength, Izod notched, ASTM

394 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 394 J/m

Tensile strength

197.0 MPa

Show Supplier Material materials with Tensile strength of 197.0 MPa

Thermal

PropertyValuePressureComment

Heat deflection temperature

90.0 °C

Show Supplier Material materials with Heat deflection temperature of 90.0 °C

1.8 MPa

ASTM D648

Rheological Properties

PropertyValue

Shrinkage

0.1 %

Show Supplier Material materials with Shrinkage of 0.1 %

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

Technological properties

Property
Application areas

Automotive and Hand Tools.

Fillers

50% Long Glass Fiber