TPU 8101LGF60

Alternative and trade names
8101LGF60
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 8101LGF60 is a long glass fiber reinforced. ISOTHANE 8102LGF60 exhibits excellent tensile and flexural strength, toughness,abrasive resistance, high rigidity, and maintenance of good physical properties under UV exposure. ISOTHANE 8102LGF60 can be injection molded and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.7 g/cm³

Show Supplier Material materials with Density of 1.7 g/cm³

Mechanical

PropertyTemperatureValue

Flexural modulus

23.0 °C

13.3 GPa

Show Supplier Material materials with Flexural modulus of 13.3 GPa

Flexural strength

23.0 °C

335 MPa

Show Supplier Material materials with Flexural strength of 335 MPa

Impact strength, Izod notched, ASTM

23.0 °C

295 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 295 J/m

Tensile strength

23.0 °C

222 MPa

Show Supplier Material materials with Tensile strength of 222 MPa

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

95 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 95 °C

ASTM D648

Rheological Properties

PropertyTemperatureValue

Shrinkage

23.0 °C

0.05 - 0.2 %

Show Supplier Material materials with Shrinkage of 0.05 - 0.2 %

Technological properties

Property
Application areas

Automotive and Hand Tools.

Fillers

60% Long Glass Fiber