ABS 525

Alternative and trade names
ABS525
Want to keep this datasheet? Save it now in your required format

Description

High ridigity

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.04 g/cm³

Show Supplier Material materials with Density of 1.04 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Flexural modulus

2.55 GPa

Show Supplier Material materials with Flexural modulus of 2.55 GPa

ASTM D790

Flexural strength

80.0 MPa

Show Supplier Material materials with Flexural strength of 80.0 MPa

ASTM D790

Hardness, Rockwell R

110.0 [-]

Show Supplier Material materials with Hardness, Rockwell R of 110.0 [-]

ASTM D785

Impact strength, Izod notched, ASTM

176.4 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 176.4 J/m

ASTM D256

Yield strength

51.0 MPa

Show Supplier Material materials with Yield strength of 51.0 MPa

ASTM D638

Thermal

PropertyValuePressureComment

Heat deflection temperature

90.0 °C

Show Supplier Material materials with Heat deflection temperature of 90.0 °C

1.8 MPa

ASTM D648

Vicat softening temperature

95.0 °C

Show Supplier Material materials with Vicat softening temperature of 95.0 °C

ASTM D1525, 1kg load

Flammability

UL94 HB

Rheological Properties

PropertyValueComment

Melt mass-flow rate

20.0 g/10min

Show Supplier Material materials with Melt mass-flow rate of 20.0 g/10min

ASTM D1238, 220°C,10kg/cm2

Technological properties

Property
Application areas

Electronics, Household appliances