PC+ABS 625W

Alternative and trade names
PC/ABS625W
Want to keep this datasheet? Save it now in your required format

Description

High flow

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyValueComment

Flexural modulus

2.13 GPa

Show Supplier Material materials with Flexural modulus of 2.13 GPa

ASTM D790

Flexural strength

85.0 MPa

Show Supplier Material materials with Flexural strength of 85.0 MPa

ASTM D790

Hardness, Rockwell R

70.0 [-]

Show Supplier Material materials with Hardness, Rockwell R of 70.0 [-]

ASTM D785

Impact strength, Izod notched, ASTM

637 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 637 J/m

ASTM D256

Yield strength

53.0 MPa

Show Supplier Material materials with Yield strength of 53.0 MPa

ASTM D638

Thermal

PropertyValuePressureComment

Heat deflection temperature

88.0 °C

Show Supplier Material materials with Heat deflection temperature of 88.0 °C

1.8 MPa

ASTM D648

Flammability

UL94 HB

Rheological Properties

PropertyValueComment

Melt mass-flow rate

15.0 g/10min

Show Supplier Material materials with Melt mass-flow rate of 15.0 g/10min

ASTM D1238, 260°C,2.16kg

Technological properties

Property
Application areas

Automibile interior parts, Consumer electronic products, General molding products