PC+ABS 640W

Alternative and trade names
PC/ABS640W
Want to keep this datasheet? Save it now in your required format

Description

High flow

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

2.5 GPa

Show Supplier Material materials with Flexural modulus of 2.5 GPa

ASTM D790

Flexural strength

23.0 °C

84.5 MPa

Show Supplier Material materials with Flexural strength of 84.5 MPa

ASTM D790

Hardness, Rockwell R

23.0 °C

118 [-]

Show Supplier Material materials with Hardness, Rockwell R of 118 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

490 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 490 J/m

ASTM D256

Yield strength

23.0 °C

58 MPa

Show Supplier Material materials with Yield strength of 58 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

93 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 93 °C

ASTM D648

Vicat softening temperature

110 °C

Show Supplier Material materials with Vicat softening temperature of 110 °C

ASTM D1525, 1kg load

Flammability

UL94 V0 (3.2-3.5mm)

Rheological Properties

PropertyValueComment

Melt mass-flow rate

20 g/10min

Show Supplier Material materials with Melt mass-flow rate of 20 g/10min

ASTM D1238, 260°C,2.16kg

Technological properties

Property
Application areas

Automibile interior parts, Consumer electronic products, General molding products