ISOTHANE 3065A-C is a thermoplastic polyurethane for coating applicatons. ISOTHANE 3065A-C exhibits excellent mechanical properties, abrasive resistance, and easy process. ISOTHANE 3065A-C can be processed by extrusion and calendering.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.15 g/cm³

Show Supplier Material materials with Density of 1.15 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

800.0 %

Show Supplier Material materials with Elongation of 800.0 %

ASTM D412

Hardness, Shore A

65.0 [-]

Show Supplier Material materials with Hardness, Shore A of 65.0 [-]

ASTM D2240

Tear strength

42.0 kN/m

Show Supplier Material materials with Tear strength of 42.0 kN/m

ASTM D624

Tensile strength

15.0 MPa

Show Supplier Material materials with Tensile strength of 15.0 MPa

ASTM D412

Technological properties

Property
Application areas

Synthetic Leather, Furniture, Sports and Recreations.