TPU 3090A-C

Alternative and trade names
3090A-C
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 3090A-C is a thermoplastic polyurethane for coating applicatons. ISOTHANE 3090A-C exhibits excellent mechanical properties, abrasive resistance, and easy process. ISOTHANE 3090A-C can be processed by extrusion and calendering.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

450 %

Show Supplier Material materials with Elongation of 450 %

ASTM D412

Hardness, Shore A

23.0 °C

90 [-]

Show Supplier Material materials with Hardness, Shore A of 90 [-]

ASTM D2240

Tear strength

23.0 °C

96 kN/m

Show Supplier Material materials with Tear strength of 96 kN/m

ASTM D624

Tensile strength

23.0 °C

23 MPa

Show Supplier Material materials with Tensile strength of 23 MPa

ASTM D412

Technological properties

Property
Application areas

Synthetic Leather, Furniture, Sports and Recreations.