TPU G1075AU

Alternative and trade names
G1075AU
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE® G1075AU is a high performance environment-friendly TPU based on renewable materials with various bio-based content. It exhibits excellent transparency, mechanical properties, abrasive resistance and solvent resistance. ISOTHANE® G1075AU can be processed by extrusion and/or injection molding. This product contains 46% biorenewable content.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Bio-based content

46.0 %

Show Supplier Material materials with Bio-based content of 46.0 %

Density

1.21 g/cm³

Show Supplier Material materials with Density of 1.21 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Elongation

1100.0 %

Show Supplier Material materials with Elongation of 1100.0 %

ASTM D412

Hardness, Shore A

75.0 [-]

Show Supplier Material materials with Hardness, Shore A of 75.0 [-]

ASTM D2240

Tear strength

100.0 kN/m

Show Supplier Material materials with Tear strength of 100.0 kN/m

ASTM D624

Tensile strength

15.0 MPa

Show Supplier Material materials with Tensile strength of 15.0 MPa

ASTM D412

Technological properties

Property
Application areas

Packaging Material, Footwear, Consumer Goods, Automotive