General
Property | Value | Comment |
---|---|---|
Bio-based content | 25.0 % Show Supplier Material materials with Bio-based content of 25.0 % | |
Density | 1.18 g/cm³ Show Supplier Material materials with Density of 1.18 g/cm³ | ASTM D792 |
Mechanical
Property | Value | Comment |
---|---|---|
Elongation | 570.0 % Show Supplier Material materials with Elongation of 570.0 % | ASTM D412 |
Hardness, Shore A | 95.0 [-] Show Supplier Material materials with Hardness, Shore A of 95.0 [-] | ASTM D2240 |
Tear strength | 195.0 kN/m Show Supplier Material materials with Tear strength of 195.0 kN/m | ASTM D624 |
Tensile strength | 51.0 MPa Show Supplier Material materials with Tensile strength of 51.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |