Hera 648 (PdAgCuPtAu alloy)

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Heraeus.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

11.8 g/cm³

Show Supplier Material materials with Density of 11.8 g/cm³

Dimension

PropertyValue

Dimensions

Dimensions available upon request.

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

108 GPa

Show Supplier Material materials with Elastic modulus of 108 GPa

Elongation

23.0 °C

3 %

Show Supplier Material materials with Elongation of 3 %

max.

Hardness, Vickers

23.0 °C

330 - 400 [-]

Show Supplier Material materials with Hardness, Vickers of 330 - 400 [-]

Shear modulus

23.0 °C

40 GPa

Show Supplier Material materials with Shear modulus of 40 GPa

Tensile strength

23.0 °C

1100 - 1400 MPa

Show Supplier Material materials with Tensile strength of 1100 - 1400 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.46E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.46E-5 1/K

RT-100 °C

Melting point

1130 - 1180 °C

Show Supplier Material materials with Melting point of 1130 - 1180 °C

Thermal conductivity

23.0 °C

28 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 28 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

3.38E-7 - 3.59E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 3.38E-7 - 3.59E-7 Ω·m

Specific Electrical conductivity

4.8 - 5.1 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 4.8 - 5.1 % IACS

Temperature coefficient of resistance

23.0 °C

2.8E-4 1/K

Show Supplier Material materials with Temperature coefficient of resistance of 2.8E-4 1/K

Technological properties

Property
Application areas

Sliding contacts, Slip ring brushes, Potentiometers, probe pins

Corrosion properties

Corrosion resistant

Other

Superb sliding contact alloy, stable contact resistance, wear resistant, Oxidation resistant up to 300 °C, Ductile