General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 14.3 g/cm³ Show Supplier Material materials with Density of 14.3 g/cm³ |
Dimension
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 124 GPa Show Supplier Material materials with Elastic modulus of 124 GPa | |
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | max. |
Hardness, Vickers | 23.0 °C | 280 - 350 [-] Show Supplier Material materials with Hardness, Vickers of 280 - 350 [-] | |
Shear modulus | 23.0 °C | 44 GPa Show Supplier Material materials with Shear modulus of 44 GPa | |
Tensile strength | 23.0 °C | 900 - 1150 MPa Show Supplier Material materials with Tensile strength of 900 - 1150 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.41E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.41E-5 1/K | RT-100 °C |
Melting point | 1190 - 1230 °C Show Supplier Material materials with Melting point of 1190 - 1230 °C | ||
Thermal conductivity | 23.0 °C | 31 W/(m·K) Show Supplier Material materials with Thermal conductivity of 31 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 2.87E-7 - 3.13E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 2.87E-7 - 3.13E-7 Ω·m |
Specific Electrical conductivity | 5.5 - 6 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5.5 - 6 % IACS | |
Temperature coefficient of resistance | 23.0 °C | 1.8E-4 1/K Show Supplier Material materials with Temperature coefficient of resistance of 1.8E-4 1/K |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding contacts, Slip ring brushes | |
Corrosion properties | Corrosion resistant | |
Other | Oxidation resistant, Ductile, Age hardenable, Wear Resistant, stable contact resistant |