Hera 238 (AuAgCu alloy)

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Heraeus.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

15.1 g/cm³

Show Supplier Material materials with Density of 15.1 g/cm³

Dimension

PropertyValue

Dimensions

Dimensions available upon request.

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

87 GPa

Show Supplier Material materials with Elastic modulus of 87 GPa

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

min.

Hardness, Vickers

23.0 °C

120 - 170 [-]

Show Supplier Material materials with Hardness, Vickers of 120 - 170 [-]

Shear modulus

23.0 °C

37 GPa

Show Supplier Material materials with Shear modulus of 37 GPa

Tensile strength

23.0 °C

400 - 600 MPa

Show Supplier Material materials with Tensile strength of 400 - 600 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.67E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.67E-5 1/K

RT-100 °C

Melting point

865 - 895 °C

Show Supplier Material materials with Melting point of 865 - 895 °C

Thermal conductivity

23.0 °C

66 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 66 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.25E-7 - 1.45E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.25E-7 - 1.45E-7 Ω·m

Specific Electrical conductivity

11.9 - 13.8 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 11.9 - 13.8 % IACS

Temperature coefficient of resistance

23.0 °C

5.2E-4 1/K

Show Supplier Material materials with Temperature coefficient of resistance of 5.2E-4 1/K

Technological properties

Property
Application areas

Sliding contacts, Slip ring brushes, Resistance wires

Corrosion properties

Corrosion resistant

Other

Wear resistant, Age hardenable, Ductile, High electrical conductivity, Stable Contact resistant