AgCu20

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Heraeus.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

10.13 g/cm³

Show Supplier Material materials with Density of 10.13 g/cm³

Dimension

PropertyValue

Dimensions

Dimensions available upon request.

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

85 GPa

Show Supplier Material materials with Elastic modulus of 85 GPa

Elongation

23.0 °C

20 %

Show Supplier Material materials with Elongation of 20 %

min.

Hardness, Vickers

23.0 °C

80 - 120 [-]

Show Supplier Material materials with Hardness, Vickers of 80 - 120 [-]

Tensile strength

23.0 °C

300 - 400 MPa

Show Supplier Material materials with Tensile strength of 300 - 400 MPa

Yield strength Rp0.2

23.0 °C

200 - 300 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 200 - 300 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.93E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.93E-5 1/K

RT-100 °C

Melting point

779 - 820 °C

Show Supplier Material materials with Melting point of 779 - 820 °C

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

2.2E-8 - 2.5E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 2.2E-8 - 2.5E-8 Ω·m

Specific Electrical conductivity

70 - 77 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 70 - 77 % IACS

Temperature coefficient of resistance

23.0 °C

4.3E-4 1/K

Show Supplier Material materials with Temperature coefficient of resistance of 4.3E-4 1/K

Technological properties

Property
Application areas

Sliding contacts, Slip ring brushes, switching contacts

Corrosion properties

Corrosion resistant

Other

Ductile, High conductivity, Low contact resistance, Susceptible to attack by sulphur