IrRh10

Want to keep this datasheet? Save it now in your required format

Properties

General

Density

ρ

20.7 g/cm³ at 23 °C

Dimension

Dimensions

Dimensions available upon request.

Mechanical

Hardness, Vickers

HV

200 - 550 [-] at 23 °C

Show Iridium materials with Hardness, Vickers of 200 - 550 [-] at 23 °C

Technological properties

Application areas

Spark plugs

Corrosion properties

Corrosion resistant

Other

Erosion resistant, temperature stable

This material data has been provided by Heraeus.