PtRh5 DPH

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Heraeus.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

20.59 g/cm³

Show Supplier Material materials with Density of 20.59 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

106 GPa

Show Supplier Material materials with Elastic modulus of 106 GPa

Elongation

20.0 °C

39 %

Show Supplier Material materials with Elongation of 39 %

1200.0 °C

59 %

Show Supplier Material materials with Elongation of 59 %

1400.0 °C

68 %

Show Supplier Material materials with Elongation of 68 %

1600.0 °C

71 %

Show Supplier Material materials with Elongation of 71 %

Hardness, Vickers

23.0 °C

82 [-]

Show Supplier Material materials with Hardness, Vickers of 82 [-]

Tensile strength

20.0 °C

290 MPa

Show Supplier Material materials with Tensile strength of 290 MPa

1200.0 °C

55.3 MPa

Show Supplier Material materials with Tensile strength of 55.3 MPa

1400.0 °C

31.2 MPa

Show Supplier Material materials with Tensile strength of 31.2 MPa

1600.0 °C

19.2 MPa

Show Supplier Material materials with Tensile strength of 19.2 MPa

Unlock all property charts

Yield strength Rp0.2

20.0 °C

128 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 128 MPa

1200.0 °C

40 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 40 MPa

1400.0 °C

27 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 27 MPa

1600.0 °C

16.1 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 16.1 MPa

Unlock all property charts

Thermal

PropertyTemperatureValue

Thermal conductivity

20.0 °C

45.2 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 45.2 W/(m·K)

1200.0 °C

72.6 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 72.6 W/(m·K)

1400.0 °C

74.7 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 74.7 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

1.7E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.7E-7 Ω·m

1146.0 °C

5.3E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.3E-7 Ω·m

1369.0 °C

6E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 6E-7 Ω·m

Unlock all property charts