PA66 ISO-TECH

Alternative and trade names
ISO-MID PA66
Want to keep this datasheet? Save it now in your required format

This material data has been provided by ISO-TECH Kunststoff GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.14 g/cm³

Show Supplier Material materials with Density of 1.14 g/cm³

ISO 1183

Water absorption

23.0 °C

2.8 %

Show Supplier Material materials with Water absorption of 2.8 %

ISO 62

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.1 GPa

Show Supplier Material materials with Elastic modulus of 3.1 GPa

ISO 527

Elongation

23.0 °C

40 %

Show Supplier Material materials with Elongation of 40 %

ISO 527

Hardness, Ball Indentation

23.0 °C

170 MPa

Show Supplier Material materials with Hardness, Ball Indentation of 170 MPa

ISO 2039-1

Yield strength

23.0 °C

80 MPa

Show Supplier Material materials with Yield strength of 80 MPa

ISO 527

Impact strength, Charpy unnotched

No break, ISO 179

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K

DIN 53752

Heat deflection temperature, 0.45 MPa

200 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C

Heat deflection temperature, 1.80 MPa

100 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 100 °C

Max service temperature

100 °C

Show Supplier Material materials with Max service temperature of 100 °C

Longterm

Min service temperature

-30 °C

Show Supplier Material materials with Min service temperature of -30 °C

Longterm

Thermal conductivity

23.0 °C

0.23 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.23 W/(m·K)

DIN 52612

Flammability

HB UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112

Dielectric constant, 1MHz

23.0 °C

3.6 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 3.6 [-]

DIN 53483

Dielectric strength

23.0 °C

30 kV/mm

Show Supplier Material materials with Dielectric strength of 30 kV/mm

VDE 0303

Loss tangent, 1MHz

23.0 °C

0.03 [-]

Show Supplier Material materials with Loss tangent, 1MHz of 0.03 [-]

DIN 53483

Surface resistivity

23.0 °C

1.00E+10 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+10 Ω/sq

min., VDE 0303

Volume resistivity

23.0 °C

1.00E+12 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+12 Ω·cm

min., VDE 0303

Technological properties

Property
Certifications

RoHS,REACH

UV resistance

Partly