PA6 ISO-TECH

Alternative and trade names
ISO-MID PA 6
Want to keep this datasheet? Save it now in your required format

Description

ISO-MID PA 6 is a semi-crystalline thermoplastic, which has proven itself particularly by its favourable characteristics at high temperatures. Due to its balanced mechanical properties, ISO-MID PA 6 is widely used as a material for sliding bearings, rollers or gears. The key features are:


  • Good damping and abrasion characteristics
  • Higher temperature resistance
  • Low length expansion at temperature fluctuations
  • Good machinability
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueComment

    Coefficient of friction

    0.35 [-]

    Show Supplier Material materials with Coefficient of friction of 0.35 [-]

    DIN 53375, D, Against dry running steel

    Density

    1.15 g/cm³

    Show Supplier Material materials with Density of 1.15 g/cm³

    ISO 1183

    Water absorption

    2.2 %

    Show Supplier Material materials with Water absorption of 2.2 %

    ISO 62

    Mechanical

    PropertyValueComment

    Elastic modulus

    3 GPa

    Show Supplier Material materials with Elastic modulus of 3 GPa

    ISO 527

    Elongation

    40 %

    Show Supplier Material materials with Elongation of 40 %

    ISO 527

    Flexural strength

    140 MPa

    Show Supplier Material materials with Flexural strength of 140 MPa

    ISO 178

    Hardness, Ball Indentation

    160 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 160 MPa

    ISO 2039-1

    Hardness, Shore D

    82 [-]

    Show Supplier Material materials with Hardness, Shore D of 82 [-]

    DIN 53505

    Impact strength, Charpy notched

    4 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m²

    min., ISO 179

    Yield strength

    80 MPa

    Show Supplier Material materials with Yield strength of 80 MPa

    ISO 527

    Impact strength, Charpy unnotched

    No break, ISO 179

    Thermal

    PropertyValueComment

    Coefficient of thermal expansion

    8e-05 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 8e-05 1/K

    DIN 53752

    Max service temperature

    105 °C

    Show Supplier Material materials with Max service temperature of 105 °C

    Longterm

    Long

    Short

    Min service temperature

    -40 °C

    Show Supplier Material materials with Min service temperature of -40 °C

    Longterm

    Thermal conductivity

    0.23 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.23 W/(m·K)

    DIN 52612

    Flammability

    HB UL 94

    Electrical

    PropertyValueComment

    Dielectric constant

    3.7 [-]

    Show Supplier Material materials with Dielectric constant of 3.7 [-]

    DIN 53483

    Dielectric strength

    50 kV/mm

    Show Supplier Material materials with Dielectric strength of 50 kV/mm

    VDE 0303

    Loss tangent

    0.03 [-]

    Show Supplier Material materials with Loss tangent of 0.03 [-]

    DIN 53483

    Surface resistivity

    1e+13 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq

    min., VDE 0303

    Volume resistivity

    1e+15 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1e+15 Ω·cm

    min., VDE 0303

    Technological properties

    Property
    Application areas

    Sliding parts, rollers and impact stressed parts

    Certifications

    Food Contact: FDA and EU 10/2011, RoHS,REACH