PA6G + OIL ISO-TECH

Alternative and trade names
ISO-MID PA6G+Oil
Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ISO-TECH Kunststoff GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Coefficient of friction

0.3 [-]

Show Supplier Material materials with Coefficient of friction of 0.3 [-]

DIN 53375, C, Against dry running steel

Density

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

ISO 1183

Water absorption

0.2 %

Show Supplier Material materials with Water absorption of 0.2 %

ISO 62

Mechanical

PropertyValueComment

Elastic modulus

3 GPa

Show Supplier Material materials with Elastic modulus of 3 GPa

ISO 527

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527

Elongation at yield

8 %

Show Supplier Material materials with Elongation at yield of 8 %

ISO 527

Flexural strength

95 MPa

Show Supplier Material materials with Flexural strength of 95 MPa

ISO 178

Hardness, Ball Indentation

150 MPa

Show Supplier Material materials with Hardness, Ball Indentation of 150 MPa

ISO 2039-1

Hardness, Shore D

85 [-]

Show Supplier Material materials with Hardness, Shore D of 85 [-]

DIN 53505

Impact strength, Charpy notched

5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

min., ISO 179

Tear strength

60 kN/m

Show Supplier Material materials with Tear strength of 60 kN/m

ISO 527

Yield strength

66 MPa

Show Supplier Material materials with Yield strength of 66 MPa

ISO 527

Impact strength, Charpy unnotched

No break, ISO 179

Thermal

PropertyValueComment

Coefficient of thermal expansion

8e-05 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8e-05 1/K

DIN 53752

Max service temperature

100 °C

Show Supplier Material materials with Max service temperature of 100 °C

Longterm

Long

Short

Min service temperature

-40 °C

Show Supplier Material materials with Min service temperature of -40 °C

Longterm

Thermal conductivity

0.37 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.37 W/(m·K)

DIN 52612

Flammability

HB UL 94

Electrical

PropertyValueComment

Comparative tracking index

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112

Dielectric strength

50 kV/mm

Show Supplier Material materials with Dielectric strength of 50 kV/mm

VDE 0303

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

min., VDE 0303

Volume resistivity

1e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+14 Ω·cm

min., VDE 0303

Technological properties

Property
Application areas

Sliding parts, rollers and impact stressed parts

Certifications

RoHS,REACH